The invention relates to a bamboo deep-processing product and a process method, in particular a processing process for the production of bamboo fibers by physical and chemical methods.
OBJECTS OF THE INVENTION It is an object of the present invention to provide a method for extracting natural bamboo fibers having a diameter of 0.03-0.4mm and a length of 10-250mm, which are different from bamboo fibers which are generally in the form of thick, short or block blocks, and also different from polymeric bamboo fibers which are blended with other fibers in the textile industry.
The basic principle of the production process of the invention is to use the original bamboo (bamboo chips) by physical and chemical method, in alkaline solution to soften, de-sugar, de-fat, protein, starch treatment, by mechanical impact, tear, open into bamboo fiber.
The process of the invention is the original bamboo cutting and cracking, softening treatment, opening into fiber, washing and bleaching, dehydration drying, screening and packaging into storage.
The specific production process of the present invention is as follows: A. Any bamboo is selected for cutting and cracking of the original bamboo; The original bamboo or bamboo slices are broken and cut into sheets or plate reticulate of not less than 50mm by manual or mechanical means; B, softening treatment The bamboo slices are softened in lye, and sugar, fat, lignin and the like in some bamboo are removed at the same time, and the softened bamboo slices are yellow; the method includes the first method of putting bamboo chips into a cooking container, adding alkali or liquid ammonia and diluting with water, the concentration of the solution is controlled at 1-20%, the liquid level is more than 1mm higher than the bamboo chips, and cooking at 1-6 atmospheric pressure for more than 5 minutes, and the cooking temperature is above 90 ℃;
Method 2 Put bamboo slices into a soaking tank and add a solution containing alkali or liquid ammonia for soaking. The concentration of the solution is not less than 1%, the liquid level is more than 1mm higher than the bamboo slices, and the soaking time is more than 10 hours. Method 3 Soak the bamboo slices with lime water, spread a layer of lime in the soaking tank, and finally add water to the bamboo surface so that the water can completely submerge the bamboo slices for more than 7 days, the amount of lime in the soaking tank is more than 5% of the water volume; C, the bamboo chips softened by the opening fiber are torn by impact on the nail type bamboo fiber extractor to open bamboo fibers containing residual alkali and bamboo powder; D. washing and bleaching bamboo fibers are put into a washing tank and washed with clear water, then sent to a bleaching tank for bleaching with bleaching solution under stirring, and washed with clear water flow again to obtain white bamboo fibers; the bleaching solution is calcium hypochlorite solution, sodium hypochlorite solution, potassium hypochlorite solution, or hydrogen peroxide solution, or chlorine gas is directly introduced into the bleaching tank. The concentration of bleaching solution is above 0.01, the solution temperature is above 1 ℃, and the bleaching time is above 5 minutes. Bamboo fibers that have not been bleached only after washing are yellow. E. Dehydration and Drying After dewatering the washed bamboo fibers by mechanical drying method or vacuum method or plate pressing method, it is sent to a dryer for drying or natural drying under sunlight. After drying, the moisture content of bamboo fiber is 3-30%. F. Sieving, packing, storage and drying bamboo fibers are sent to a vibrating screening machine for screening to remove thick and short fibers, bamboo stalks, bamboo joints, bamboo heads, bamboo powder and long and short fibers that have not been completely opened, to obtain fibers that meet the requirements of bamboo fiber standards and package them into finished products.
The product standard 1 of the present invention is yellow in appearance color. The diameter is 0.03-0.4mm and the length is 10-250mm; 2, no impurities, insect corrosion, mildew; 3, moisture control in 3-30%;4, bamboo powder, bamboo stem, bamboo head content is not more than 15%;5, residual alkali content (1Kg of fiber finished product into 24 ℃,10Kg of pure water soaking for 8 hours, water leaching alkali) s 5g The process method of the present invention is suitable for the production of glass fiber substitutes and sewage treatment filter inner material, through the use of effect comparison analysis, this product can fully meet the performance requirements, but also has a high environmental protection value, and low economic cost.